Alloy EN 43200 or GALSi10 is relatively simple to use and requires general attention typical of foundry aluminum alloys. EN standard requires Mg as an alloying element to make it capable of responding to heat treatment.
Elem. | % Min | % Max |
---|---|---|
Si | 9,0 | 11,0 |
Fe | 0,55 | |
Cu | 0,3 | |
Mn | 0,55 | |
Mg | 0,25 | 0,45 |
Cr | - | |
Ni | 0,15 | |
Zn | 0,35 | |
Pb | 0,10 | |
Sn | - | |
Ti | 0,15 | |
Impurezze singole | 0,05 | |
Impurezze globali | 0,15 |